Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 316 g/mol | 316 g/mol | Theoretical, approximate |
PolyOne reFlex™ 100 Plasticizer, Bio-derived Bio-derived, non-phthalate plasticizer; USDA BioPreferred® certified 94% biobased.Information provided by PolyOne |
|||
Molecular Weight | 316 g/mol | 316 g/mol | |
3M Novec™ 649 Engineered Fluid 3M™ Novec™ 649 Engineered Fluid is a clear, colorless and low odor fluid, one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high global.. |