Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1045 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1080 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1250 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1500 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1700 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 - 5.00e+6 g/mol | 3.00e+6 - 5.00e+6 g/mol | |
Inhance Fluoro-Seal INHANCE® UH-1900 Ultra High Molecular Weight Polyethylene Product Description: INHANCE UH-1000 series particles are surface-activated Ultra High Molecular Weight Polyethylene (UHMWPE) in powder form. Surface activation makes the particles easy to disperse.. |
|||
Molecular Weight | 3.00e+6 g/mol | 3.00e+6 g/mol | Braskem |
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene Description: UTEC3040 is an Ultra High Molecular Weight Polyethylene with a molecular weight about 10 times higher than High Density Polyethylene (HDPE) resins. This extremely high molecular weight .. |
|||
Molecular Weight | 3.00e+6 g/mol | 3.00e+6 g/mol | Braskem |
Braskem UTEC® 3041 Ultra High Molecular Weight Polyethylene Applications which require high impact resistance and use of pigments and/or additives - filters, technical and porous parts, compression molded sheets.Information provided by Braskem. |
|||
Molecular Weight | 3.00e+6 - 4.00e+6 g/mol | 3.00e+6 - 4.00e+6 g/mol | |
Beijing Evergrow Resources UHMW PE Powder Ultra-high molecular weight polyethylene (UHMWPE) is an outstanding engineering plastic. It’s characterized by the following properties.Features:Very high abrasion resistanceVery high impact streng.. |