Beijing Evergrow Resources UHMW PE Powder

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Beijing Evergrow Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources UHMW PE Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultra-high molecular weight polyethylene (UHMWPE) is an outstanding engineering plastic. It’s characterized by the following properties.Features:Very high abrasion resistanceVery high impact strengthVery low coefficient frictionGood self-lubricantExcellent resistance to chemicalsGood resistance to low temperatureExcellent dielectric properties Information provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Bulk Density 0.450 g/cc
0.0163 lb/in³
Density 0.935 g/cc
0.0338 lb/in³
Volatiles <= 0.15 %
<= 0.15 %
Moisture
Particle Mesh Size 20 Mesh
20 Mesh
1% retained
Molecular Weight 3.00e+6 - 4.00e+6 g/mol
3.00e+6 - 4.00e+6 g/mol
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa

@Temperature 32.0 °C
5080 psi

@Temperature 89.6 °F
Elongation at Break 200 - 300 %
200 - 300 %
Izod Impact, Unnotched NB
NB
Izod Impact, Notched (ISO) >= 70.0 kJ/m²
>= 33.3 ft-lb/in²
Thermal Properties Metric English Comments
Heat Distortion Temperature >= 80.0 °C
>= 176 °F