Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 2650 g/mol | 2650 g/mol | |
BASF Pluronic® 17 R4 Block Copolymer Surfactant Description: Pluronic 17R4 is a difunctional block copolymer surfactant with terminal secondary hydroxyl groups. A nonionic surfactant that is 100% active and relatively non-toxic.Information provi.. |