Material Notes:
Description: Pluronic 17R4 is a difunctional block copolymer surfactant with terminal secondary hydroxyl groups. A nonionic surfactant that is 100% active and relatively non-toxic.Information provided by BASF
Physical Properties Metric English Comments
Density 1.048 g/cc
0.03786 lb/in³
Solubility in Water >= 10 %
>= 10 %
pH 5.5 - 6.7
5.5 - 6.7
2.5% aqueous
Viscosity 600 cP
600 cP
Molecular Weight 2650 g/mol
2650 g/mol
Surface Tension 44 dynes/cm
44 dynes/cm
Thermal Properties Metric English Comments
Pour Point 18.0 °C
64.4 °F
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Color <80
APHA