Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 136 g/mol | 136 g/mol | |
Dow Corning Z-6070 SILANE Dow Corning Z-6070 Silane is a chemical monomer that reacts with water to form a silanetriol and methanol. The silanol that is formed is able to condense with available hydroxyl groups on the surfac.. |