Material Notes:
Dow Corning Z-6070 Silane is a chemical monomer that reacts with water to form a silanetriol and methanol. The silanol that is formed is able to condense with available hydroxyl groups on the surface of inorganic minerals such as talc, clay and silica or to condense with other silanol monomers to form a siloxane resin. The chemical formula of Dow Corning Z-6070 Silane is (CH3O)3SiCH3, which is designated methyltrimethoxysilane.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc

@Temperature 25.0 °C
0.950 g/cc

@Temperature 77.0 °F
Molecular Weight 136 g/mol
136 g/mol
Thermal Properties Metric English Comments
Flash Point 8.00 °C
46.4 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.37
1.37
Processing Properties Metric English Comments
Shelf Life 36.0 Month
36.0 Month
Descriptive Properties Value Comments
Appearance colorless, clear
Hydrophobic yes
Purity (%) 95
Users viewing this material also viewed the following: