Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 104.2 g/mol | 104.2 g/mol | |
BASF 1,2-Pentanediol Formula: C5H12O2CAS: 5343-92-0Description: 1,2-Pentanediol is a colorless to yellowish liquid, with a pungent odor. It is miscible with water.Synonyms: Pentane-1,2-diolApplications: Intermediate us.. |
|||
Molecular Weight | 104.2 g/mol | 104.2 g/mol | |
BASF 1,5-Pentanediol (PDO) Formula: C5H12O2CAS: 111-29-5Description: 1,5-Pentanediol (PDO) is a colorless, oily liquid with characteristic odor. It is miscible in water and organic solvents.Synonyms: 1,5-Dihydroxypentane, 1,5.. |
|||
Molecular Weight | 104.2 g/mol | 104.2 g/mol | |
BASF NEOL® Neolpentylglycol Flakes Formula: C5H12O2CAS: 126-30-7Description: Neolpentylglycol (NEOL) flakes are colorless with a sweetish odor.Synonyms: Neopentanediol, 2,2-Dimethyl-1,3-propanediol, 1,3-Dihydroxy-2,2-dimethylpropane,.. |
|||
Molecular Weight | 104.2 g/mol | 104.2 g/mol | |
BASF NEOL® Neolpentylglycol Pure Liquid Formula: C5H12O2CAS: 126-30-7Description: Neolpentylglycol (NEOL) pure liquid is a colorless melt, with a sweetish odor. Synonyms: Neopentanediol, 2,2-Dimethyl-1,3-propanediol, 1,3-Dihydroxy-2,2-dim.. |
|||
Molecular Weight | 104.2 g/mol | 104.2 g/mol | |
BASF NEOL® Neopentylglycol 90% Solution Formula: C5H12O2CAS: 126-30-7Description: Neol 90% solution is colorless and partially crystalline, with a sweet odor. It is very soluble in water.Applications: Intermediate used in the production .. |