Material Notes:
Formula: C5H12O2CAS: 5343-92-0Description: 1,2-Pentanediol is a colorless to yellowish liquid, with a pungent odor. It is miscible with water.Synonyms: Pentane-1,2-diolApplications: Intermediate used in the production of Crop Protection Agents and PesticidesInformation provided by BASF
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Molecular Weight 104.2 g/mol
104.2 g/mol
Thermal Properties Metric English Comments
Melting Point <= -40.0 °C
<= -40.0 °F
Boiling Point 208 - 210 °C
406 - 410 °F
Flash Point 110 °C
230 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
DIN 51 777
Descriptive Properties Value Comments
Assay >98%
Ignition Temperature 380°C