Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 52 m²/g | 52 m²/g | |
BASF Heligoen® Blue L 6875 H Color Additive Description: Reddish a-phthalocyanine blue with excellent flocculation resistance and dispersibility.Chemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking system.. |
|||
Specific Surface Area | 52 m²/g | 52 m²/g | |
BASF Paliogen® Blue L 6470 Color Additive Description: Transparent Indanthrone blue for effect and solid shades with high fastness propertiesPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, A.. |