BASF Heligoen® Blue L 6875 H Color Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Heligoen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Heligoen® Blue L 6875 H Color Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Reddish a-phthalocyanine blue with excellent flocculation resistance and dispersibility.Chemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems, and Airdrying systems.Information provided by BASF
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0603 lb/in³
Specific Surface Area 52 m²/g
52 m²/g
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 350 °C
662 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 5000 ohm-cm
>= 5000 ohm-cm
Chemical Properties Metric English Comments
Total Acid Number 4.0 - 7.0
4.0 - 7.0
Descriptive Properties Value Comments
Chemical Fastness (months) Butylacetate
3
Ethanol
3-4
HCL 2%
5
Methyl ethyl ketone
1
Mineral spirits
4-5
NaOH 2%
5
Solvenon™PM
2
Xylene
3
Color Blue
Fastness to Overcoating 4-5