Polymer Property : Specific Surface Area = 24 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 24 m²/g
24 m²/g
Imerys Hamiltonâ„¢ Kaolin
Hamilton is a fine-grained kaolin with low alkali content and high PCE. These properties make for ideal air-set refractory mortars. Halloysite content provides excellent suspension and trowel abilit..