Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 18.3 m²/g | 18.3 m²/g | |
Old Hickory FC-120 Tennessee Ball Clay The FC-120 clay is a special selection for sanitaryware. It is very fast casting and is designed to use in combination with the C-33A or other finer particle size distribution clay. The FC-120 provi.. |