Polymer Property : Specific Surface Area = 15.0 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 15.0 m²/g
15.0 m²/g
BET
KaMin Polyplate® P Kaolin Clay - Delaminated
Polyplate® P is a high brightness, delaminated clay intended for use in latex paints, water flexography inks, water-based adhesives or water-based systems where increased hiding, tinting strength..
Specific Surface Area 15.0 m²/g
15.0 m²/g
BET
KaMin Polyplate® P01 Kaolin Clay - Delaminated
Polyplate® P01 is a milled, high brightness, large particle size delaminated kaolin, intended for use in solvent and water-borne coatings, inks, and adhesives. The high aspect ratio of the large ..
Specific Surface Area 15.0 m²/g
15.0 m²/g
BET
KaMin Polyfil® DL Kaolin Clay - Delaminated
Large, platy delaminated clay that reduces gas/vapor permeability, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, MasterBatchInform..
Specific Surface Area 15.0 m²/g
15.0 m²/g
BET
KaMin Polyfil® WC-426 Kaolin Clay - Calcined
Fine particle size vinyl-functional calcined clay for outstanding wet electricals and long term stability in wire and cable applications.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rub..