Polymer Property : Specific Surface Area = 1100 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 1100 m²/g
1100 m²/g
BET
Beijing Evergrow Resources ACFC1100 Activated Carbon Fiber Cloth
Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral content Applicati..
Specific Surface Area 1100 m²/g
1100 m²/g
BET
Beijing Evergrow Resources ACFCC-1100 Activated Carbon Fiber Composite Cloth
Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplicatio..