Physical Properties Metric English Comments
Particle Size 9500 µm
9500 µm
Zeon Chemicals Nipol® 1472X Nitrile Powder and Crumb Elastomer
Nipol 1472X is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile contnet modified to contain carboxyl groups. It contains sufficient antioxidant for normal storage conditions. ..
Particle Size 9500 µm
9500 µm
Zeon Chemicals Nipol® 1401LG Nitrile Powder and Crumb Elastomer
Nipol 1401LG is a copolymer of butadiene and acrylonitrile of excellent oil resistance. This material is ground and dusted with approximately 2.0% mineral anticake which allows direct addition to mi..
Particle Size 9500 µm
9500 µm
Zeon Chemicals Nipol® 1432T Nitrile Powder and Crumb Elastomer
Nipol 1432T is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile content. Sufficient antioxidant is added during manufacture for normal storage conditions.Used in adhesives and..
Particle Size 9500 µm
9500 µm
Zeon Chemicals Nipol® 1442 Nitrile Powder and Crumb Elastomer
Nipol 1442 is a copolymer of butadiene and acrylonitrile with medium-high acrylonitrile content. Nipol 1442 shall be in the form of nominal 1/4" three-dimensional chips containing approximately 5%mi..
Particle Size 9500 µm
9500 µm
Zeon Chemicals Nipol® 1472HV Nitrile Powder and Crumb Elastomer
Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is ..