Polymer Property : Particle Size = 500 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 200 - 500 µm
200 - 500 µm
Polimeri Europa Extir® F 1111 Expandable Polystyrene  (discontinued **)
Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont..
Particle Size 200 - 500 µm
200 - 500 µm
Polimeri Europa Extir® P 1212 Expandable Polystyrene  (discontinued **)
Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. ..
Particle Size 125 - 500 µm
125 - 500 µm
Average value: 283 µm Grade Count:3
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Particle Size 200 - 500 µm
200 - 500 µm
GB/T 12005.7
Lushan DE-1 Polyethylene Sintered Powder
PE sintered powder Lushan DE-1 is combined with more than 10 years practice and experience on the area of oil & gas pipeline anti-corrosion. PE sintered powder Lushan DE-1 is used on anti-corrosion ..
Particle Size 200 - 500 µm
200 - 500 µm
GB/T 12005.7
Lushan DP-1 Polypropylene sintered powder, Ultra Fast Cure
PP sintered powder Lushan DP-1 is used on anti-corrosion coated steel pipe Polypropylene top coats and applied in oil & gas submarine counterweight pipeline to make a non-slid surface to avoid skidd..
Particle Size 200 - 500 µm
200 - 500 µm
Dry
Shamrock Technologies NanoFLON® P 39B Thermoplastic Grade PTFE Additive
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro..
Particle Size 200 - 500 µm
200 - 500 µm
Dry
Shamrock Technologies NanoFLON® P 40A Thermoplastic Grade PTFE Additive
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro..
Particle Size 200 - 500 µm
200 - 500 µm
Dry
Shamrock Technologies NanoFLON® P 47A Thermoplastic Grade PTFE Additive
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro..
Particle Size 200 - 500 µm
200 - 500 µm
Dry
Shamrock Technologies NanoFLON® P 63B Thermoplastic Grade PTFE Additive
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro..
Particle Size 10 - 500 µm
10 - 500 µm
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres
EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t..
Particle Size 10 - 500 µm
10 - 500 µm
SPHERE ONE EXTENDOSPHERESâ„¢ HA Hollow Spheres
EXTENDOSPHERESâ„¢ HA are off white, low-cost, low-density, high alumina, ceramic hollow spheres.Applications: Hollow spheres are ideal for use in coatings, sealants, caulks and other applications..
Particle Size 10 - 500 µm
10 - 500 µm
SPHERE ONE EXTENDOSPHERESâ„¢ SG Hollow Spheres
EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t..
Particle Size 200 - 500 µm
200 - 500 µm
Dry
Shamrock Technologies NanoFLON® P 51A Thermoplastic Grade PTFE Additive
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro..
Particle Size 5.0 - 500 µm
5.0 - 500 µm
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Particle Size 5.0 - 500 µm
5.0 - 500 µm
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Particle Size 10 - 500 µm
10 - 500 µm
Solvay MIRAPOL® SURF-S PFREE POWER Surfactant
Description: Blend of acrylic based polymer and sodium carbonate. This polymer is used as a rinse-aid agent to replace the nonionic surfactant 3-in-1 product in automatic dish wash. It is very effic..