Lushan DP-1 Polypropylene sintered powder, Ultra Fast Cure

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Lushan
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lushan DP-1 Polypropylene sintered powder, Ultra Fast Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP sintered powder Lushan DP-1 is used on anti-corrosion coated steel pipe Polypropylene top coats and applied in oil & gas submarine counterweight pipeline to make a non-slid surface to avoid skidding. PP sintered powder Lushan DP-1 is combined with more than 10 years practice and experience on the area of oil & gas pipeline anti-corrosion. PP sintered powder Lushan DP-1 has good stability, wide processing technology, strong adhesion with the outer PP layer, high mechanical strength and ageing resistance property, etc.Information provided by Lushan
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
GB/T1033.1
Particle Size 200 - 500 µm
200 - 500 µm
GB/T 12005.7
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.0 MPa
3190 psi
GB/T1040.1
Flexural Modulus 0.600 GPa
87.0 ksi
GB/T94341
Processing Properties Metric English Comments
Moisture Content 0.050 %
0.050 %
HG/T2751