Polymer Property : Particle Size = 3150 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 100 - 3150 µm
100 - 3150 µm
Average value: 1110 µm Grade Count:47
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Particle Size 2200 - 3150 µm
2200 - 3150 µm
SYNTHOS Koplen® 2040 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO ..
Particle Size 2200 - 3150 µm
2200 - 3150 µm
SYNTHOS Koplen® 2040 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks. Lower density can be achieved after several prefor..