Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1700 - 2800 µm | 1700 - 2800 µm | min 92%; BC HSZ 326:2001/1 screening |
BorsodChem ONGROSTYR F-IV Expandable Polystyrene (EPS) ONGROSTYR F-IV is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e.. |