Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1700 - 2300 µm | 1700 - 2300 µm | |
Potters Industries A-Series A-205 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 1700 - 2800 µm | 1700 - 2800 µm | min 92%; BC HSZ 326:2001/1 screening |
BorsodChem ONGROSTYR F-IV Expandable Polystyrene (EPS) ONGROSTYR F-IV is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e.. |