Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1.0 - 2.2 µm | 1.0 - 2.2 µm | d50 |
Magyar Aluminum ALOLT 60DLS Aluminum Hydroxide Fine Precipitated Type |
|||
Particle Size | 1.0 - 2.2 µm | 1.0 - 2.2 µm | d50 |
Magyar Aluminum ALOLT 60F Aluminum Hydroxide Fine Precipitated Type |
|||
Particle Size | 1.0 - 2.2 µm | 1.0 - 2.2 µm | d50 |
Magyar Aluminum ALOLT 60P Aluminum Hydroxide Fine Precipitated Type |