Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2.12 µm | 2.12 µm | Median particle diameter |
Old Hickory UltraCast Slurry PC-2000 Kentucky Ball Clay These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c.. |