Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
Nabaltec NABALOX® NO 615-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
Nabaltec NABALOX® NO 625-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
Nabaltec NABALOX® NO 625-31 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
d50
Magyar Aluminum ALOLT 90DLS Aluminum Hydroxide
Fine Precipitated Type
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
d50
Magyar Aluminum ALOLT 90F Aluminum Hydroxide
Fine Precipitated Type
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
FSSS
H.C. Starck Ampersint® MAP FeCoNi 40/20/40 For Hardmetals
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
FSSS
H.C. Starck Ampersint® MAP FeCoNi 70/10/20 For Hardmetals
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
FSSS
H.C. Starck Ampersint® MAP FeNi 50/50 For Hardmetals
High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a ..
Particle Size 1.3 - 2.0 µm
1.3 - 2.0 µm
Average
H.C. Starck Grade B Titanium Carbonitride
Hard metals (tooling and machining)CermetsBlack ceramics
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
Laser Diffraction D50
H.C. Starck Grade I Amorphous Boron
Automotive (igniter in airbags and belt tighteners)Additive in pyrotechnic mixtures (flares, igniters, and delay compositions)Additive in solid rocket propellant fuels and explosivesPreparation of r..
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
Laser Diffraction D50
H.C. Starck Grade C Titanium Carbonitride
Hard metals (tooling and machining)CermetsBlack ceramics
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
Laser Diffraction D50
H.C. Starck Grade C Titanium Nitride
Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets
Particle Size 0.20 - 2.0 µm
0.20 - 2.0 µm
Dispersed
Shamrock Technologies NanoFLON® P 63B Thermoplastic Grade PTFE Additive
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro..
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
D50 Sedigraph
Solvay CEROXâ„¢ 1650 Surfactant
Description: Ceroxâ„¢1650 offers an optimized polishing performance for optical and ophthalmic lenses as well as for other demanding applications like photomask and glass hard disks. Benefits: Hi..
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
D50 Sedigraph
Solvay SUPER CEROXâ„¢ 1663 Surfactant
Description: Super Ceroxâ„¢1663 is particularly suited for the polishing of ophthalmic lenses (mass production and prescription) and optical lenses. Benefits: High polishing efficiency, Very high..