Physical Properties Metric English Comments
Particle Size 10 - 15 µm
10 - 15 µm
d50
Magyar Aluminum ALOLT 8AF Aluminum Hydroxide
Ground type
Particle Size 7.0 - 15 µm
7.0 - 15 µm
average
Malvern Minerals Novacite® 325 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Particle Size 7.0 - 15 µm
7.0 - 15 µm
average
Malvern Minerals Novakup® 325 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Particle Size 11 - 15 µm
11 - 15 µm
10%
H.C. Starck Amperit® 151.065 Tantalum (Ta)
Particle Size 11 - 15 µm
11 - 15 µm
10%
H.C. Starck Amperit® 161.065 Niobium (Nb)
Particle Size 10 - 15 µm
10 - 15 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade A Silicon Hexaboride, SiB6
Particle Size 10 - 15 µm
10 - 15 µm
10%
H.C. Starck Amperit® 140.3 Tungsten (W)
HS Number: 81011000
Particle Size 10 - 15 µm
10 - 15 µm
10%
H.C. Starck Amperit® 146.3 Chromium (Cr)
HS Number: 81122031
Particle Size 9.0 - 15 µm
9.0 - 15 µm
d90, Guaranteed
TIMCAL TIMREX® LSG10 Natural Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Particle Size 10 - 15 µm
10 - 15 µm
China Tungsten YG13C Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 10 - 15 µm
10 - 15 µm
China Tungsten YG15C Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 10 - 15 µm
10 - 15 µm
China Tungsten YG6C Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 10 - 15 µm
10 - 15 µm
China Tungsten YG11C Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 10 - 15 µm
10 - 15 µm
China Tungsten YG9C Tungsten Carbide Powder
Information provided by China Tungsten
Particle Size 9.0 - 15 µm
9.0 - 15 µm
D(0.5)
Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 9.0 - 15 µm
9.0 - 15 µm
D(0.5)
Akzo Nobel Expancel® 461 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 9.0 - 15 µm
9.0 - 15 µm
D(0.5)
Akzo Nobel Expancel® 461 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 9.0 - 15 µm
9.0 - 15 µm
D(0.5)
Akzo Nobel Expancel® 051 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..