Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 120 - 130 µm | 120 - 130 µm | Mean |
SPHERE ONE EXTENDOSPHERESâ„¢ SLG Hollow Spheres EXTENDOSPHERESâ„¢ SL are white, low-cost, low-density ceramic hollow spheres.Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in.. |
|||
Particle Size | 20 - 130 µm | 20 - 130 µm | D10-D90 |
ALM TPE-210-S Prototyping Polymer A thermoplastic elastomer used to produce parts with “rubber like” qualities. TPE 210-S exhibits good feature definition and infiltration with polyurethane will impart even higher toughness and ab.. |
|||
Particle Size | 120 - 130 µm | 120 - 130 µm | mean diameter |
BCC Products BC 37 Ceramic Microspheres BC 37 are hollow microspheres, which are ceramic in nature. They are an efficient lightweight filler material to be used in applications with most resins.Information provided by BCC Products, Inc. |