Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1.1 µm | 1.1 µm | |
Imerys Alumex™ Kaolin Alumex is a Hydrated Aluminum Silicate used as a low surface area “soft†filler for Elastomeric systems.Information provided by Imerys |
|||
Particle Size | 1.1 µm | 1.1 µm | average |
Imerys Kaolexâ„¢ FG Kaolin Kaolex FG is a air floated Hydrated Aluminum Silicate. Its low surface area makes it a good choice for fiberglass manufacturing.Information provided by Imerys |
|||
Particle Size | 1.1 µm | 1.1 µm | average |
Imerys Kaolexâ„¢ SC Kaolin Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.Information provided by Imerys |
|||
Particle Size | 1.1 µm | 1.1 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade B7 Silicon Nitride, Si3N4 Alpha phase > 87%Ceramic cutting toolsHeavy duty components in automotive enginesHigh performance parts for mechanical engineeringBearing components, like high precision ballsSiAlONsMetallurgy (ther.. |
|||
Particle Size | 1.1 - 3.0 µm | 1.1 - 3.0 µm | d50 |
Indium Corp. Fine ITO Indium Tin Oxide Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo.. |
|||
Particle Size | 1.1 - 7.2 µm | 1.1 - 7.2 µm | d90 |
Indium Corp. In(OH)3 Fine Indium Hydroxide Indium Acetate is a white powder. Fine Powder Form: Primary particles range from 0.1 to 1.0 microns in size. they range in shape from spherical to elliptical to cylindrical. Agglomerates can be .. |
|||
Particle Size | 1.1 - 2.6 µm | 1.1 - 2.6 µm | d50 |
Indium Corp. In2O3 Type B Indium Oxide, Fine Powder Indium Sesquioxide is a yellow colored powder. It is a stable ceramic-like material, insoluble in water and volatizes at 850°C. Indium sesquioxide is a n-type semiconductor and as such is used .. |