Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.65 µm | 0.65 µm | Median particle diameter |
Old Hickory 56-SR Kentucky Ball Clay This is a kaolinitic clay with excellent extrusion and die pressing characteristics. It has some colloidal carbon content but only a moderate amount of shrinkage. This clay is suitable for a variety.. |
|||
Particle Size | 0.65 µm | 0.65 µm | Median particle diameter |
Old Hickory S-4 Tennessee Ball Clay The S-4 clay is designed for all types of casting formulas ranging from low fire earthenware to vitreous compositions. It has excellent response to deflocculation and very good casting rate while ma.. |