Material Notes:
This is a kaolinitic clay with excellent extrusion and die pressing characteristics. It has some colloidal carbon content but only a moderate amount of shrinkage. This clay is suitable for a variety of refractory compositions or other ceramic formulations such as stoneware.Information provided by Old Hickory Clay Company
Physical Properties Metric English Comments
Particle Size 0.50 µm
0.50 µm
48% of particles less than
0.65 µm
0.65 µm
Median particle diameter
1.0 µm
1.0 µm
60% of particles less than
<= 5.0 µm
<= 5.0 µm
85% of particles less than
pH 5.0
5.0
Soluble Sulfates 350 ppm
350 ppm
Specific Surface Area 20.3 m²/g
20.3 m²/g
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00414 GPa
0.600 ksi
Dry Modulus of Rupture for 50% clay/50% flint, cast bars
Thermal Properties Metric English Comments
Shrinkage 4.7 %
4.7 %
Cone 04, Linear Fired Shrinkage
4.9 %
4.9 %
Cone 3, Linear Fired Shrinkage
6.6 %
6.6 %
Cone 11, Linear Fired Shrinkage
7.0 %
7.0 %
Linear Drying Shrinkage
Component Elements Properties Metric English Comments
Al2O3 27.99 %
27.99 %
CaO 0.15 %
0.15 %
Fe2O3 1.1 %
1.1 %
K2O 0.69 %
0.69 %
Loss on Ignition(%) 10.31 %
10.31 %
MgO 0.34 %
0.34 %
Na2O 0.080 %
0.080 %
SiO2 57 %
57 %
TiO2 2.1 %
2.1 %
Descriptive Properties Value Comments
Absorption (%) 11.6
Cone 04, Fired
4.3
Cone 11, Fired
9.4
Cone 3, Fired
CEC/MBI (meg/100 ml) 8.7
Crude Color Brown
Filtration (ml) 22
Pyrometric Cone Equivalent (PCE) 32
Water of Plasticity (%) 33
Wet Sieve Residue (%) 1.04
Wet Sieve Residue, +200 mesh
Copyright © lookpolymers.com All Rights Reserved