Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.35 µm | 0.35 µm | Median |
Nabaltec ACTILOX® 200 AS1 AlO(OH) Boehmite Surface treated flame retardant filler with reduced particle size and optimized viscosity in engineering plastics for synergistic effects with other flame retardants.Properties:Very fine product in .. |
|||
Particle Size | 0.35 µm | 0.35 µm | Median; Laser Diffraction |
Nabaltec ACTILOX® 200SM AlO(OH) Boehmite Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature stabilitySynergistic effects with other flame retardantsHigh acid resistance.. |