Polymer Property : Particle Size = 0.35 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.35 µm
0.35 µm
Median
Nabaltec ACTILOX® 200 AS1 AlO(OH) Boehmite
Surface treated flame retardant filler with reduced particle size and optimized viscosity in engineering plastics for synergistic effects with other flame retardants.Properties:Very fine product in ..
Particle Size 0.35 µm
0.35 µm
Median; Laser Diffraction
Nabaltec ACTILOX® 200SM AlO(OH) Boehmite
Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature stabilitySynergistic effects with other flame retardantsHigh acid resistance..