Polymer Property : Particle Size = 0.22 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.22 µm
0.22 µm
Primary; Internal Method
Solvay Specialty Polymers Algoflon® L203 Polytetrafluoroethylene (PTFE)  (Unverified Data**)
Algoflon® L203 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It is recommended for use as an additive in high quality oils and greases to reduce coefficie..
Particle Size 0.22 µm
0.22 µm
Mallard Creek Polymers ROVENE® 4049 SBR Latex
ROVENE® 4049 is a carboxylated styrene-butadiene emulsion that has a medium hand with above average strength properties. This binder has the ability to be cross-linked with external cross-linking..
Particle Size 0.22 µm
0.22 µm
Mallard Creek Polymers ROVENE® 4402 SBR Latex
ROVENE® 4402 is a carboxylated styrene-butadiene emulsion which does not contain nor evolve formaldehyde during cure. ROVENE® 4402 has a medium soft hand with outstanding strength properties. ..
Particle Size 0.22 µm
0.22 µm
Mallard Creek Polymers Rovene® 6506 Styrene-Acrylic Emulsion
Applications: Rovene® 6506 typical applications are across a variety of nonwoven markets and substrates. Rovene® 6506 has demonstrated excellent performance as a binder on a lightweight nonwov..
Particle Size 0.22 µm
0.22 µm
average; DIN ISO 13321
3M Dyneon™ TF 5035Z PTFE
Due to its good film-forming properties 3M™ Dyneon™ PTFE TF 5035Z is an excellent choice for formulating aqueous non-stick coating systems, which can be used to coat suitably prepared metal, glass..