Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.010 - 0.15 µm | 0.010 - 0.15 µm | |
American Elements Silicon Carbide Nanoparticles General DescriptionSilicon Carbide (SiC) Nanoparticles, whiskers, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Carbide Particles are typically 10 - 150 nanomet.. |