Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

American Elements Silicon Carbide Nanoparticles

Category Ceramic , Carbide
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Silicon Carbide Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionSilicon Carbide (SiC) Nanoparticles, whiskers, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Carbide Particles are typically 10 - 150 nanometers (nm) with specific surface area (SSA) in the 10 – 75 m 2 /g range. Nano Silicon Carbide Particles are also available in ultra high purity and high purity and coated and dispersed forms. Research into applications for Silicon Carbide nanocrystals includes use as a dielectric coating, in solar cell applications, as a high temperature insulator, as a gas sensor and for use in other coatings, plastics, polymers and wire.
Physical Properties Metric English Comments
Particle Size 0.010 - 0.15 µm
0.010 - 0.15 µm
Specific Surface Area 10 - 75 m²/g
10 - 75 m²/g
Descriptive Properties Value Comments
Appearance Silvery
Users viewing this material also viewed the following: