Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | outside diameter |
NanoAmor 90%, OD/ID: 10-30/3-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 10-30/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.030 µm | 0.020 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 20-30/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.030 µm | 0.020 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID: 20-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.030 µm | 0.0050 - 0.030 µm | wall thickness |
NanoAmor 95%, OD/WT/L: 40-70/5-30 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.030 µm | 0.020 - 0.030 µm | outside diameter |
NanoAmor 95%, OD: 20-30 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.030 µm | 0.020 - 0.030 µm | outside diameter |
NanoAmor 95%, OD: 20-30 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.030 µm | 0.0050 - 0.030 µm | wall thickness |
NanoAmor 99%, OD/WT/L: 40-70/5-30 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID: 10-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Aluminum Nanoparticles General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Lanthanum Oxide Nanopowder General DescriptionLanthanum Oxide (LaO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Lanthanum Oxide Particles are typically 10-30 nanomete.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Nickel Oxide Nanopowder General DescriptionNickel Oxide (NiO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Nickel Oxide Particles are typically 10-30 nanometers (nm.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Vanadium Oxide Nanopowder General DescriptionVanadium Oxide (VO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Vanadium Oxide Particles are typically 10-30 nanometers .. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Chromium Oxide Nanopowder General DescriptionChromium Oxide (CrO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Chromium Oxide Particles are typically 10-30 nanometers.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Cobalt Oxide Nanopowder General DescriptionCobalt Oxide (CoO) Nanoparticles, nanodots or nanopowder are white spherical high surface area metal particles. Nanoscale Cobalt Oxide Particles are typically 10-30 nanometers (nm.. |
|||
Particle Size | 0.010 - 0.030 µm | 0.010 - 0.030 µm | |
American Elements Copper Nanoparticles General DescriptionCopper (Cu) Nanoparticles, nanodots or Nanopowder are black brown spherical high surface area metal particles. Nanoscale Copper Particles are typically 10-30 nanometers (nm) with .. |
|||
Particle Size | 0.0010 - 0.030 µm | 0.0010 - 0.030 µm | |
American Elements Copper Oxide Nanopowder General DescriptionCopper Oxide (CuO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Copper Oxide Particles are typically 1-30 nanometers (nm).. |