Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD/ID/L: 30-50/5-15 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD/ID/L: 50-80/5-15 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0080 - 0.015 µm | 0.0080 - 0.015 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 8-15/3-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0080 - 0.015 µm | 0.0080 - 0.015 µm | outside diameter |
NanoAmor 95%, OD/ID: 8-15/3-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | wall thickness |
NanoAmor 95%, OD/WT/L: 20-40/5-15 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD: 30-50 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD: 30-50 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD: 50-80 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD: 50-80 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0080 - 0.015 µm | 0.0080 - 0.015 µm | outside diameter |
NanoAmor 95%, OD: 8-15 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0080 - 0.015 µm | 0.0080 - 0.015 µm | outside diameter |
NanoAmor 95%, OD: 8-15 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD/ID: 30-50/5-15 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD/ID: 50-80/5-15 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |