NanoAmor 95%, OD: 50-80 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes

Category Carbon
Manufacturer Nanostructured & Amorphous Materials Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoAmor 95%, OD: 50-80 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and shieldingEnergy conversionLithium-battery anodesHydrogen storageNanotube composites (by filling or coating);Nanoprobes for STM, AFM, and EFM tips, nanolithography, nanoelectrodes, drug delivery, sensorsReinforcements in compositesSupercapacitorInformation provided by NanoAmor Inc.
Physical Properties Metric English Comments
Particle Size 0.0050 - 0.015 µm
0.0050 - 0.015 µm
inside diameter
0.050 - 0.080 µm
0.050 - 0.080 µm
outside diameter
Specific Surface Area 40 m²/g
40 m²/g
Descriptive Properties Value Comments
Color black
Content of -COOH wt% 1 to 6
Length (um) 10-20
Mole fraction of surface carbon atoms 8 to 10
Purity (vol% carbon nanotubes), min 95