Polymer Property : Particle Size = 0.0011 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.0011 µm
0.0011 µm
Average, from Raman Spectra
NanoAmor 50% Regular Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an..