Physical Properties Metric English Comments
Particle Size 0.00080 - 0.0016 µm
0.00080 - 0.0016 µm
from Raman Spectra
NanoAmor 50% Regular Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an..