Physical Properties Metric English Comments
Bulk Density 7.10 g/cc
0.257 lb/in³
Sintered
TIMCAL TIMREX® F10 Primary Synthetic P/M Special-Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..