Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18A Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18B Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18C Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18CX Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18D Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18DX Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories FAM-1 Flame-Gunning Repair Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories FAM-2 Flame-Gunning Repair Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.92 g/cc | 0.105 lb/in³ | |
Chosun Refractories C18AX Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |