Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.58 g/cc | 0.0932 lb/in³ | |
Chosun Refractories CRAG-S50 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.58 g/cc | 0.0932 lb/in³ | |
Chosun Refractories CRAG-S50 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.58 g/cc | 0.0932 lb/in³ | |
Chosun Refractories H-1 High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |