Polymer Property : Bulk Density = 2.40 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable
This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt..
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 160 HC Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s..
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Gouda Vuurvast FLUCON 140 Dense Self Flowing Refractory Castable
Description: Flucon 140 is a self flowing low cement castable, based on a high quality chamotte grog.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable
Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar..
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable
Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 160 H Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc..
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
Sharadaa Ceramics LI SILL-I High Alumina Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 165 GM Dense Refractory Castable
Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo..