Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.85 - 1.95 g/cc | 0.0668 - 0.0704 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 100 Dense Refractory Castable Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modification.. |
|||
Bulk Density | 1.85 - 1.95 g/cc | 0.0668 - 0.0704 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 100 C Dense Refractory Castable Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values .. |