Polymer Property : Bulk Density = 1.57 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.57 g/cc
0.0567 lb/in³
Tapped; ASTM D 3101-78
Potters Industries Spheriglass® 1922 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Bulk Density 1.57 g/cc
0.0567 lb/in³
Tapped; ASTM D 3101-78
Potters Industries Spheriglass® 2024 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Bulk Density 1.57 g/cc
0.0567 lb/in³
Tapped; ASTM D 3101-78
Potters Industries Spheriglass® 2429 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Bulk Density 1.57 g/cc
0.0567 lb/in³
Tapped; ASTM D 3101-78
Potters Industries Spheriglass® 2530 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Bulk Density 1.57 - 1.67 g/cc
0.0567 - 0.0603 lb/in³
3M #11 Roofing Granule (Pittsboro)
3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre..