Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.57 g/cc | 0.0567 lb/in³ | Tapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 1922 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Bulk Density | 1.57 g/cc | 0.0567 lb/in³ | Tapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 2024 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Bulk Density | 1.57 g/cc | 0.0567 lb/in³ | Tapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 2429 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Bulk Density | 1.57 g/cc | 0.0567 lb/in³ | Tapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 2530 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Bulk Density | 1.57 - 1.67 g/cc | 0.0567 - 0.0603 lb/in³ | |
3M #11 Roofing Granule (Pittsboro) 3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre.. |