Polymer Property : Bulk Density = 1.50 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.50 g/cc
0.0542 lb/in³
Oceanchem Group Melamine Polyphosphate (MPP)
Cas No.: 20208-95-1Use: Mainly used in polyamide and PBT, especially PA6, PA66, glass fiber-reinforced PA6, PA66. Nylon containing FR-NP can be used in all kinds of injection and extrusion processe..
Bulk Density 1.50 g/cc
0.0542 lb/in³
packed
Omya PULPROWHITE® 3 - SA Calcium Carbonate
A dry ground calcium carbonate with excellent fineness and dispersion characteristics.Information supplied by Omya North America.
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP1000 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP125 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP80 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP850 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP860 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP1500 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP2000 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
MarkeTech Repton 201 Aluminum Oxide
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
Bulk Density 1.50 g/cc
0.0542 lb/in³
MarkeTech Repton 632 Mullite
Brand 632 features: Light Weight Setter.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when th..
Bulk Density 1.50 g/cc
0.0542 lb/in³
MarkeTech Repton 902 Cordierite Mg-Al-Si Oxide
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
Bulk Density 1.50 - 1.60 g/cc
0.0542 - 0.0578 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 145 Refractory Insulating Castable
Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also avail..
Bulk Density 1.50 g/cc

@Temperature 200 °C
0.0542 lb/in³

@Temperature 392 °F
Sharadaa Ceramics Sharada LTM 1.5 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Bulk Density 1.50 g/cc
0.0542 lb/in³
Zircar Zirconia ZHB Zirconia Hollow Balls
Zirconia Hollow Balls Type ZHB are sintered calcia-stabilized zirconia hollow balls, which flow easily into a confined space. Our standard product is our Type ZHB-1 which ranges in particle size fro..
Bulk Density >= 1.50 g/cc
>= 0.0542 lb/in³
Chosun Refractories HL-18 Special Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 1.50 g/cc
0.0542 lb/in³
Chosun Refractories CC-1 Blast Furnace Tap-Hole Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 1.50 g/cc
0.0541 lb/in³
Powder
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina
Fine grain castable for potting and producing small tools.
Bulk Density 1.50 g/cc
0.0542 lb/in³
3M W-210 Ceramic Microspheres
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l..
Bulk Density 1.50 g/cc
0.0542 lb/in³
3M W-410 Ceramic Microspheres
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l..
Bulk Density 1.50 g/cc
0.0542 lb/in³
3M W-610 Ceramic Microspheres
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP18 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP300 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP40 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP600 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP780 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 - 1.60 g/cc
0.0542 - 0.0578 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable
Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Bulk Density 1.50 g/cc
0.0542 lb/in³
Zircar Zirconia ZHB Zirconia Hollow Balls
Zirconia Hollow Balls Type ZHB are sintered calcia-stabilized zirconia hollow balls, which flow easily into a confined space. Our standard product is our Type ZHB-1 which ranges in particle size fro..
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
PPT BP125HR NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Bulk Density 1.50 - 1.60 g/cc
0.0542 - 0.0578 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable
Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere...