Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.28 g/cc | 0.0463 lb/in³ | Untapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 5000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Bulk Density | 1.28 g/cc | 0.0462 lb/in³ | |
Inhance Fluoro-Seal INHANCE® Si-8500 Polymer Alloy Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with v.. |
|||
Bulk Density | 1.28 g/cc | 0.0463 lb/in³ | Loose |
Excalibar ExCal® 100 Calcium Carbonate CaCO3 Powder ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli.. |
|||
Bulk Density | 1.28 g/cc | 0.0463 lb/in³ | Packed |
Excalibar ExCal® 200 Calcium Carbonate CaCO3 Powder ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli.. |
|||
Bulk Density | 1.28 g/cc | 0.0463 lb/in³ | |
ATI Wah Chang Jet Milled Zirconium Oxide, ZrO2 Jet Milled. A fine, white powder.Information provided by ATI Wah ChangTypical Analysis: On Zr oxide basis |