Polymer Property : Bulk Density = 0.881 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman Aqua 20837 PET  (discontinued **)
Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 15041 PET  (discontinued **)
Voridian polymer 15041 is a PET thermoplastic polyester.Applications/UsesCrystallized PET (CPET) trays
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 7352 PET  (discontinued **)
VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 9663 PET  (discontinued **)
VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 9921 PET Injection Molded  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 9921P PET Film  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 9921P PET Injection Molded  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Bulk Density 0.881 g/cc
0.0318 lb/in³
packed
Imerys Minsparâ„¢ 7 Ground Feldspar
Minsparâ„¢ 7 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 7 is easily dispersed to a high Hegman grind to produce coatings with hig..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Loose
Excalibar ExBar™ W 1 Barite BaSO4 Powder
ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, ..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Loose
Excalibar ExCal® 325 Calcium Carbonate CaCO3 Powder
ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
DAK Americas Laser+® MB912 PET
Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient pr..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Loose
CIMBAR FlexTalc® 815D Ultrafine Talc for TPO Applications, Densified
Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 5214A PET  (discontinued **)
Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Bulk Density 0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Eastman 9921W PET Injection Molded  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Bulk Density 0.881 g/cc
0.0318 lb/in³
ATI Wah Chang Zirconium Hydroxide, Zr(OH)4
A moist, white filter cake.Information provided by ATI Wah ChangTypical Analysis: On filter cake basis