Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.865 g/cc | 0.0312 lb/in³ | Vibrated; ASTM D1895 |
DAK Americas Laser+® HS AD600A PET Product Description: Laser+® HS (AD600A) is designed for PET packaging by injection stretch blow-molding using commercial heat-set technology. This polymer was formulated for processes requiring fa.. |
|||
Bulk Density | 0.865 g/cc | 0.0313 lb/in³ | |
3M Interam™ E-5A-4 Endothermic Mat When properly installed, 3M Interam Endothermic Mat E-5A-4 provides a uniform covering that, when exposed to high temperatures, releases chemically-bound water to cool the outer surfaces of the wrap.. |